Mark the length using spare plunger. Cut along the line, using seperating disk.
|
![]() |
![]() |
Carefull break segments apart.
Carefully sandblast
objects with glass beads. Start with 60 psi pressure, as soon as
objects appear turn pressure down to 35 psi procceed blasting
carefully.
|
![]() |
|
Carefully seperate the sprue from the objects with a sharp diamond
disk. Check the fit and finish with fine diamond burs and silicon
rubber wheels. Do not use carbide burs or high speed handpieces.
|
![]() |
![]() |
Prepare objects to desired conture (texture, contacts, etc.). Sandblast with 50µ aluminium oxide with low pressure and clean. Additions can be made, using overlay material. Customize the restoration according to situation, using Stains. This can be repeated several times. After desired effects are achieved, glaze once or twice as required. Firing is carried out on firing pillow. |
![]() |