Classic

 

Process alloys according to manufacturers instructions. Avoid sharp edges. Unless specified otherwise, the alloy should be sandblasted with min. 110µm ALOX at 2 Bar.

In most cases, especially on NP, the oxides are to be removed using min. 110µm aluminus oxide. (Refer to manufacturers manuals!)

A clean and grease-free surface must be present.

 

 
A uniform oxide layer is desired.